Sutherland Welles Ltd.® TIMBER FRAMES
Transcription
Sutherland Welles Ltd.® TIMBER FRAMES
Sutherland Welles Ltd.® Sustainable, natural & earth-friendly Polymerized Tung Oil wood finishes. INSTRUCTIONS TIMBER FRAMES Helpful Hint! We have a solution to finishing an entire post and beam project. To protect the exposed structure our Exterior Polymerized Tung Oil Sealer is a perfect beam dressing. Our line of interior finishes meet all the needs of timber frame surfaces; ceilings, beams, walls, windows, doors and floors. Sutherland Welles Ltd.® Sustainable, natural & earth-friendly Polymerized Tung Oil wood finishes. Exterior Timber Frame Wood Preparation Remove dirt from the log using a wire brush without scaring the surface. Exterior Polymerized Tung Oil Sealer The combination of UV guards, fungicide and Polymerized Tung Oil make this a superior beam dressing during construction or while the sturcture is exposed. The low solid of Polymerized Tung Oil penetrates into the green wood and allows transfer of moisture out of the log minimizing cracking. This is an alternative to a PEG solution. Applicator Options Brush: Natural white china bristle brush (thin coats only) Instructions step 1: - Apply Exterior Sealer - Don’t wipe - Let cure 12-24 hours step 2: - Apply Exterior Sealer - Don’t wipe - Let cure 24 hours 800.322.1245 & 802.635.2700 • [email protected] • P.O. Box 180 | 5575 Rte. 100 North, North Hyde Park, VT 05665 Sutherland Welles Ltd.® Sustainable, natural & earth-friendly Polymerized Tung Oil wood finishes. Interior Timber Frames Original Formula & Botanical Polymerized Tung Oil Sealer or Low Lustre These two lines are all Polymerized Tung Oil with no resin fortification. The difference in the two formulations is the solvent. The Original Formula is a petroleum solvent and the Botanical is our proprietary citrus solvent, Di-Citrusol™ They can be used interchangeably. The concept for finishing the surfaces of a timber frame structure is to keep the sheen as low and natural looking as possible. Ceiling Instructions Low Sheen step 1: - Apply Sealer - Wait 30 min. - Wipe unabsorbed finish - Let cure 6-8 hours step 2: - Sand 400 grit - Vacuum & tack surface (use Mineral Sprits on a rag to clean surface) step 3: - Apply Sealer - Wait 10-15 min. - Wipe unabsorbed finish - Let cure 24 hours Wood Preparation All wood surfaces should be free of lint, dirt, grease, wax, oil and old paint. If you are refinishing old wood, please make sure to remove any loose old finish. Sand the wood using 120/220 grit paper. Avoid using higher grits as they close down the wood pores interfering with maximum penetration. Applicator Options Rag: Scott® blue paper shop towels Brush: Natural white china bristle brush (thin coats only) Cure Test Push finger tips against the grain of the wood. If they glide easily over the surface, you are ready to apply your next coat. Post & Beam Dense Wood Instructions Low Sheen step 1: - Apply Sealer - Wait 30 min. - Wipe unabsorbed finish (If the wood is smooth) - Let cure 6-8 hours step 2: - Apply Sealer - Wait 10-15 min. - Wipe unabsorbed finish (If the wood is smooth) - Let cure 24 hours Post & Beam Porous Wood Instructions Low-Medium Sheen step 1: - Apply Low Lustre - Let cure 6-8 hours step 2: - Apply Low Lustre - Let cure 24 hours Repeat step 2 for higher sheen. Repeat step 2 for higher sheen. Repeat steps 2-3 for higher sheen. 800.322.1245 & 802.635.2700 • [email protected] • P.O. Box 180 | 5575 Rte. 100 North, North Hyde Park, VT 05665 Sutherland Welles Ltd.® Sustainable, natural & earth-friendly Polymerized Tung Oil wood finishes. Interior Timber Frames Murdoch’s Hard Sealer There are some timber frame designs that prefer a highly finished look. This is best achieved using a fortified oil such as Murdoch’s Hard Sealer. The brushed application builds a rich, uniform sheen, thus creating a finished look with uniform reflectivity. Wood Preparation All wood surfaces should be free of lint, dirt, grease, wax, oil and old paint. If you are refinishing old wood, please make sure to remove any loose old finish. Sand the wood using 120/220 grit paper. Avoid using higher grits as they close down the wood pores interfering with maximum penetration. Applicator Options Rag: Scott® blue paper shop towels Brush: Natural white china bristle brush (thin coats only) Cure Test Lightly sand several inconspicuous areas. A fine, white powder indicates that you can safely apply another coat. Ceiling Instructions Low-Medium Sheen step 1: - Apply Hard Sealer - Wait 30 min. - Wipe unabsorbed finish - Let cure 6-8 hours step 2: - Sand 400 grit - Vacuum & tack surface (use Mineral Sprits on a rag to clean surface) step 3: - Apply Hard Sealer - Wait 10-15 min. - Wipe unabsorbed finish - Let cure 24 hours step 4: - Sand 400 grit - Vacuum & tack surface Post & Beam Dense Wood Instructions Low-Medium Sheen step 1: - Apply Hard Sealer - Wait 30 min. - Wipe unabsorbed finish (If the wood is smooth) - Let cure 6-8 hours step 2: - Apply Hard Sealer - Wait 10-15 min. - Wipe unabsorbed finish (If the wood is smooth) - Let cure 24 hours Post & Beam Porous Wood Instructions Low-Medium Sheen step 1: - Apply Hard Sealer - Let cure 6-8 hours step 2: - Apply Hard Sealer - Let cure 24 hours Repeat step 2 for higher sheen. Repeat step 2 for higher sheen. (use Mineral Sprits on a rag to clean surface) step 5: - Apply Hard Sealer - Wait 10-15 min. - Wipe unabsorbed finish - Let cure 24 hours Repeat steps 4-5 for higher sheen. 800.322.1245 & 802.635.2700 • [email protected] • P.O. Box 180 | 5575 Rte. 100 North, North Hyde Park, VT 05665
Similar documents
Tung Oil - Sutherland Welles Ltd
• Vacuum: To minimize scratching vacuum regularly to keep the floor grit free. • Dust Mop: Use an oil-prepped all cotton (not synthetic) dust mop. To prep a new mop, use Sutherland Welles Ltd.® D...
More information